TY - JOUR
T1 - Effect of bimodal microstructure parameters on tensile properties, impact toughness, and deformation mechanisms of Ti80 titanium alloys
AU - Yang, Jing
AU - Zhan, Mei
AU - Wang, Qiming
AU - Sun, Guangda
AU - Li, Han
AU - Liu, Xianghong
AU - He, Yonggang
AU - Qu, Bao
AU - Lei, Fan
AU - Tuo, Liheng
AU - Zheng, Zebang
N1 - Publisher Copyright:
© 2026 Elsevier B.V.
PY - 2026/9/25
Y1 - 2026/9/25
N2 - The effects of bimodal microstructure parameters on the tensile properties, impact toughness, and underlying deformation mechanisms of Ti80 titanium alloy were systematically investigated through mechanical testing and multiscale microstructural characterization. Four distinct microstructures were produced by solution treatment at varying temperatures and cooling rates. With increasing solution temperature, the volume fraction and grain size of the primary α phase decreased progressively, while the secondary α lamella thickness was controlled by the subsequent cooling rate. Quasi-static tensile tests indicated that the bimodal microstructures exhibited superior strength (880∼893 MPa) and reduction of area (48%-50%) relative to the equiaxed microstructure. Within the bimodal microstructure, primary α content and lamella thickness had limited influence on tensile properties. In contrast, Charpy impact tests demonstrated that S3 and S4 exhibited significantly higher impact toughness,while S2 showed comparable toughness to S1, which was predominantly governed by crack propagation energy rather than crack initiation energy. Fracture surface and cross-sectional analyses revealed that the bimodal microstructures promoted more tortuous crack paths, greater crack deflection, and pronounced shear lip formation, with crack path tortuosity showing an apparent positive correlation with crack propagation energy. EBSD and TEM characterization further revealed that S4 exhibited a higher and more uniformly distributed geometrically necessary dislocation density (2.043 ×1015 m−2) and a substantially greater deformation twin fraction (47.3% {101̅2} tensile twins) relative to S1 (0.64 ×1015 m−2; below 10%). The superior impact performance of the bimodal microstructure is associated with a ‘dislocation-twin’ synergy mechanism, wherein twin-boundary-associated dislocation activity, combined with crack path deflection by the lamellar α phase, collectively expand the energy dissipation volume and enhance resistance to crack propagation under high-strain-rate loading.
AB - The effects of bimodal microstructure parameters on the tensile properties, impact toughness, and underlying deformation mechanisms of Ti80 titanium alloy were systematically investigated through mechanical testing and multiscale microstructural characterization. Four distinct microstructures were produced by solution treatment at varying temperatures and cooling rates. With increasing solution temperature, the volume fraction and grain size of the primary α phase decreased progressively, while the secondary α lamella thickness was controlled by the subsequent cooling rate. Quasi-static tensile tests indicated that the bimodal microstructures exhibited superior strength (880∼893 MPa) and reduction of area (48%-50%) relative to the equiaxed microstructure. Within the bimodal microstructure, primary α content and lamella thickness had limited influence on tensile properties. In contrast, Charpy impact tests demonstrated that S3 and S4 exhibited significantly higher impact toughness,while S2 showed comparable toughness to S1, which was predominantly governed by crack propagation energy rather than crack initiation energy. Fracture surface and cross-sectional analyses revealed that the bimodal microstructures promoted more tortuous crack paths, greater crack deflection, and pronounced shear lip formation, with crack path tortuosity showing an apparent positive correlation with crack propagation energy. EBSD and TEM characterization further revealed that S4 exhibited a higher and more uniformly distributed geometrically necessary dislocation density (2.043 ×1015 m−2) and a substantially greater deformation twin fraction (47.3% {101̅2} tensile twins) relative to S1 (0.64 ×1015 m−2; below 10%). The superior impact performance of the bimodal microstructure is associated with a ‘dislocation-twin’ synergy mechanism, wherein twin-boundary-associated dislocation activity, combined with crack path deflection by the lamellar α phase, collectively expand the energy dissipation volume and enhance resistance to crack propagation under high-strain-rate loading.
KW - Bimodal microstructure
KW - Crack propagation
KW - Deformation twinning
KW - Geometrically necessary dislocations
KW - Impact toughness
UR - https://www.scopus.com/pages/publications/105048505041
U2 - 10.1016/j.jallcom.2026.190378
DO - 10.1016/j.jallcom.2026.190378
M3 - 文章
AN - SCOPUS:105048505041
SN - 0925-8388
VL - 1080
JO - Journal of Alloys and Compounds
JF - Journal of Alloys and Compounds
M1 - 190378
ER -