摘要
Crack-free zirconia ceramics were consolidated via sintering by intense thermal radiation (SITR) approach at 1600–1700°C for 3–5 min. The resulted ceramic bulks can achieve a relative density up to 99.6% with a grain size of 300–1200 nm. Their bending strength, Vickers hardness and indentation toughness values are up to 1244 ± 139 MPa, 13.3 ± 0.3 GPa and 5.5 ± 0.1 MPa m 1/2 , respectively. Quantitative Raman and XRD analysis show the presence of minor m phase on the natural surface (<7%), fracture surface (<10%) and indentation areas (<15%). It reveals that the SITR method is efficient for rapidly manufacturing zirconia ceramics with desired density, fine grained microstructure and good mechanical properties that are strongly demanded in dental applications.
| 源语言 | 英语 |
|---|---|
| 页(从-至) | 23-29 |
| 页数 | 7 |
| 期刊 | Advances in Applied Ceramics |
| 卷 | 118 |
| 期 | 1-2 |
| DOI | |
| 出版状态 | 已出版 - 17 2月 2019 |
学术指纹
探究 'Dense and strong ZrO 2 ceramics fully densified in <15 min' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver