跳到主要导航 跳到搜索 跳到主要内容

Creep resistance limits of ZrB2/SiC composite reactively sintered from B4C and Zr5Si3 precursors

  • Dawid Kozień
  • , Wojciech Banaś
  • , Agnieszka Wojteczko
  • , Grzegorz Grabowski
  • , Alan Wilmański
  • , Paweł Nieroda
  • , Agnieszka Gubernat
  • , Ankang Li
  • , Zhouyang Li
  • , Yongsheng Liu
  • , Peter Tatarko
  • , Ondrej Hanzel
  • , Michal Hičák
  • , Chengyu Zhang
  • , Zbigniew Pędzich
  • AGH University of Krakow
  • Northwestern Polytechnical University Xian
  • Slovak Academy of Sciences

科研成果: 期刊稿件 › 文章 › 同行评审

摘要

This work investigates the high-temperature compressive creep response of a ZrB₂/SiC composite fabricated by reactive spark plasma sintering from B₄C, Zr₅Si₃, and carbon precursors. The process produced a dense two-phase composite consisting of ZrB₂ and SiC, with a fine hierarchical microstructure in which SiC occurred as intergranular regions and fine intragranular inclusions. Compressive creep tests were performed at 1300–1400°C under stresses of 100–200 MPa. The composite showed good short-term creep resistance at 1300°C, whereas testing at 1400°C under 100 MPa led to a marked increase in recorded strain and apparent late-stage creep rate. SEM observations after the 1400°C test revealed extensive cracking and local decohesion associated mainly with SiC-rich regions and ZrB₂/SiC interfaces. Thermal-stress analysis indicated that thermal-expansion mismatch between ZrB₂ and SiC contributed to damage-assisted deformation at 1400°C.

源语言英语
期刊论文编号118883
期刊Journal of the European Ceramic Society
卷47
期3
DOI
出版状态已出版 - 3月 2027

学术指纹

探究 'Creep resistance limits of ZrB2/SiC composite reactively sintered from B4C and Zr5Si3 precursors' 的科研主题。它们共同构成独一无二的学术指纹。

引用此