摘要

The authors regret there were some errors in the description of the electrode specimen thickness and the Hopkinson pressure bar diameter due to a clerical mistake. In the Fig. 1d and Table 1, due to a typo, the labels for the cathode and anode specimens were swapped. The compression test specimen was constructed from 20 stacked electrode layers, the stacking thicknesses of the anode and cathode compression samples were measured by a spiral micrometer as 3.0 mm and 2.5 mm, respectively (as shown in Table 2 of the paper). Thus, the correct labeling is shown in the Fig. 1d of this corrigendum. In Table 1, the single layer thicknesses of anode and cathode should be 150 μm and 125 μm, respectively. In the second paragraph of Section 2.1, due to the incorrect labeling of the anode and cathode sample thicknesses mentioned above, errors occurred in the calculation of the single-layer component thicknesses. Based on Table 1 and the thickness information of the current collector, the specific dimensions of the electrode’s components can be obtained. The thicknesses of active layer and current collector for the anode are 71.0 um and 8.0 um, and the thicknesses of active layer and current collector of the cathode are 55.5 um and 14.0 um, respectively. The thicknesses of current collectors were obtained from the manufacturer. It should be noted that the study presented here did not utilize these parameters. In the first paragraph of Section 2.2.2, due to a clerical error, the description of the rod diameter is incorrect. The diameter of incident bar and transmission bar of the Hopkinson pressure bar (SHPB) system should be 15 mm, as shown in Fig. 3(b) of the paper. In the original paper, the mechanical property data regarding compression and tension were derived based on the actual measured dimensions of the specimens. The specimen thickness was measured prior to each compression test (with thicknesses of 3.0 mm and 2.5 mm for the anode and cathode compression specimens, respectively), and the thickness of a single layer was derived by dividing the total thickness by the 20 stacked layers for use in processing the tensile experimental data. The errors addressed in this corrigendum arose from inadvertent slips during the writing process and do not affect the results or conclusions reported in the paper. Therefore, we hereby declare that all data, findings, discussions, and conclusions of this study remain unaffected by the corrigendum and are consistent with the original version.(Figure presented) Fig. 1. (a) Pouch cell used for the experiments. (b) Surface morphology for the two electrodes. (c) Dogbone sample prepared for tensile testing. (d) Cylindrical samples prepared for compression tests. The labels for the cathode and anode samples in Fig. 1(d) were swapped in the original paper and have now been corrected. Table 1. Material and thickness information for the electrodes used in this study.ComponentMaterialThickness (μm)AnodeGraphite/Copper150CathodeLiCoO2 /Al125The authors would like to apologise for any inconvenience caused.

源语言英语
期刊论文编号112436
期刊Engineering Fracture Mechanics
卷344
DOI
出版状态已出版 - 10 9月 2026

联合国可持续发展目标

此成果有助于实现下列可持续发展目标:

  1. 可持续发展目标 7 - 经济适用的清洁能源
    可持续发展目标 7 经济适用的清洁能源

学术指纹

探究 'Corrigendum to “Rate-dependent damage and failure behavior of lithium-ion battery electrodes”(Engineering Fracture Mechanics, (2024), 303, C, (110143), (S0013794424003060), 10.1016/j.engfracmech.2024.110143)' 的科研主题。它们共同构成独一无二的学术指纹。

引用此