Characterization of microstructure and hardness of PCVD deposited hard coatings

  • Shengli Ma
  • , Jian Xu
  • , Wanqi Jie
  • , Kewei Xu
  • , M. G.J. Veprek-Heijman
  • , S. Veprek

科研成果: 期刊稿件文章同行评审

6 引用 (Scopus)

摘要

Ti1-xAlxN hard coatings have been synthesized by direct current (dc) plasma-enhanced chemical vapor deposition (PCVD). Dependences of aluminum content and annealing at elevated temperatures on the microstructure and hardness of Ti1-xAlxN coatings were investigated. The results show that plastic hardness measured by means of indentation test increases with x increasing up to 0.83 and then decreases. XRD measurements indicate that the coatings with x < 0.83 are fcc solid solution with 3 - 10 nm grain scale. When x = 0.83, relatively soft h-AlN phase is precipitated in Ti1-xAlxN coating, while the coating hardness dramatically decreases. Furthermore, the nano-crystalline structure and high hardness of the coating can keep up to 900°C, which indicates the synthesized coating having good thermal stability.

源语言英语
页(从-至)669-672
页数4
期刊Jinshu Xuebao/Acta Metallurgica Sinica
40
6
出版状态已出版 - 6月 2004

指纹

探究 'Characterization of microstructure and hardness of PCVD deposited hard coatings' 的科研主题。它们共同构成独一无二的指纹。

引用此