TY - JOUR
T1 - Carbon Solid Solution Effect on Microstructures of Laser Powder Bed Fusion Prepared Ti Alloys
AU - Kariya, Shota
AU - Ichikawa, Eri
AU - Issariyapat, Ammarueda
AU - Umeda, Junko
AU - Chen, Biao
AU - Bahador, Abdolah
AU - Kondoh, Katsuyoshi
N1 - Publisher Copyright:
©2025 Japan Society of Powder and Powder Metallurgy.
PY - 2025
Y1 - 2025
N2 - In this study, titanium (Ti) alloy with carbon (C) solid solution was fabricated by laser powder bed fusion (LPBF) from Ti-TiC mixture powder to investigate the effect of C solid solution on microstructure and tensile properties of LPBF Ti alloy. XRD and TEM analysis showed that part of TiC particles was decomposed from the surface during melting process of LPBF and C was solid soluted in α-Ti for Ti-(0.0930.4 wt%) C. The solid solution of carbon changed the microstructure of the LPBF Ti alloy to fine acicular microstructure due to the martensitic phase transformation. This was also observed in Ti-0.4 wt% C, where solid solution of carbon was not confirmed, suggesting that in Ti-0.4 wt% C, C was once solid solution and precipitated as TiC after phase transformation. LPBF Ti-C alloys showed good strength-ductility, UTS and elongation at break for Ti-0.2 wt% C were 746 MPa and 26.3%, respectively.
AB - In this study, titanium (Ti) alloy with carbon (C) solid solution was fabricated by laser powder bed fusion (LPBF) from Ti-TiC mixture powder to investigate the effect of C solid solution on microstructure and tensile properties of LPBF Ti alloy. XRD and TEM analysis showed that part of TiC particles was decomposed from the surface during melting process of LPBF and C was solid soluted in α-Ti for Ti-(0.0930.4 wt%) C. The solid solution of carbon changed the microstructure of the LPBF Ti alloy to fine acicular microstructure due to the martensitic phase transformation. This was also observed in Ti-0.4 wt% C, where solid solution of carbon was not confirmed, suggesting that in Ti-0.4 wt% C, C was once solid solution and precipitated as TiC after phase transformation. LPBF Ti-C alloys showed good strength-ductility, UTS and elongation at break for Ti-0.2 wt% C were 746 MPa and 26.3%, respectively.
KW - TiC
KW - carbon solid solution
KW - laser powder bed fusion
KW - precipitation
KW - titanium
UR - https://www.scopus.com/pages/publications/105020015455
U2 - 10.2320/matertrans.MT-Y2025006
DO - 10.2320/matertrans.MT-Y2025006
M3 - 文章
AN - SCOPUS:105020015455
SN - 1345-9678
VL - 66
SP - 1425
EP - 1431
JO - Materials Transactions
JF - Materials Transactions
IS - 11
ER -