跳到主要导航 跳到搜索 跳到主要内容

Brazing of C/C composites and GH3044 Ni-based superalloy using Ni71CrSi as the interlayer

  • Northwestern Polytechnical University Xian

科研成果: 期刊稿件文章同行评审

7 引用 (Scopus)

摘要

C/C composites and Nickle-based superalloy GH3044 were brazed at 1 180°C for 30 min using the Ni71CrSi filler as interlayer. The wettability of filler on the surface of C/C composites and SiC modified C/C composites was studied. The microstructure, microhardness and shear fracture of the joint between C/C composites and GH3044 were investigated by scanning electron microscopy, energy-dispersive spectrometry, material universal testing machine and Micro-indentation instrument, respectively. Results showed that the joint without SiC coating got failed during the brazing process. Ni71CrSi can well braze Nickle-based superalloy and C/C composites with SiC coating. The shear strength of joint with SiC coating at room temperature was up to 35.08 MPa. The joint exhibited pseudo-plastic fracture behavior. Mechanism analysis indicated that this filler could wet modified C/C composites well. The hardness distribution of the joint presented a trend with high value at the middle and low value at the both sides, and the interfacial structure of joints was: C/C composites with SiC coating/Ni (s. s) +Cr7C3+Ni3Si/Ni (s. s) +Cr3C2+Ni3Si/Ni (s. s) +Cr3C2+MC+Ni3Si/Ni3Si+ MC +Ni (s. s) /GH3044.

源语言英语
页(从-至)665-670
页数6
期刊Materials China
32
11
DOI
出版状态已出版 - 2013

学术指纹

探究 'Brazing of C/C composites and GH3044 Ni-based superalloy using Ni71CrSi as the interlayer' 的科研主题。它们共同构成独一无二的学术指纹。

引用此