AC losses of Bi2223/Ag tapes prepared by different process

  • J. X. Wang
  • , Z. Z. Duan
  • , C. W. Yang
  • , J. N. Deng
  • , P. X. Zhang
  • , Y. F. He
  • , X. Z. Wu
  • , L. Zhou
  • Northeastern University China
  • Northwest Institute for Nonferrous Metal Research

科研成果: 期刊稿件文章同行评审

摘要

The ac losses of Bi2223/Ag tapes were measured at 77K and under alternating magnetic field(50Hz) with the peak magnitude ranges from 0. 6 to 150mT. The samples were prepared by different process. It is found that the appropriate decreasing of temperature and time of the heat treatment can reduce ac losses. The subdivision of Bi2223/Ag tapes and the reduce of the thickness can also reduce ac losses. All of these belongs to the decrease of hysteresis loss.

源语言英语
页(从-至)2603-2604
页数2
期刊Physica C: Superconductivity and its Applications
282
PART 4
DOI
出版状态已出版 - 8月 1997