跳到主要导航 跳到搜索 跳到主要内容

Ablation behavior of UHTCs carbide-modified C/C composites in extreme aerobic environments (3000℃): Evolution mechanisms of oxides film structure

  • Northwestern Polytechnical University Xian
  • Henan Academy of Sciences
  • The University of Hong Kong

科研成果: 期刊稿件 › 文章 › 同行评审

30 引用 (Scopus)

摘要

To mitigate ablation loss in carbon/carbon (C/C) composites under extreme thermal conditions (>3000℃), a novel analytical framework of “extreme environment - microstructure evolution - ablation resistance” was developed via two-way coupled simulation and multi-scale characterization. C/C-MeC-SiC (Me: Hf, Zr, Ti, Ta, Nb, W) composites were prepared by reactive melt infiltration, and the oxide film evolution of the composites under oxyacetylene ablation (4.2 MW/m2) was investigated. HfC and ZrC exhibit excellent ablation resistance by virtue of high melting points and stable oxide films (HfO2/ZrO2), but are porous due to phase transition cracks. TiC/NbC has a highly dense ceramic layer but suffers from severe ablation due to low melting point oxide loss. WC has a loose and porous oxide film due to the volatility of the oxidation products. TaSi2 is difficult to penetrate into the matrix and causes serious ablation loss. The optimized design of C/C-HfC-ZrC-TaC-SiC composites, the mass/linear variation rate were 0.175 mg/s and 0.701 μm/s after long-time ablation (1000 s, 40 s × 25 cycle), provides theoretical foundations and experimental support for the design of UHTCs modified C/C composites in extreme high-temperature environment.

源语言英语
期刊论文编号113036
期刊Corrosion Science
卷253
DOI
出版状态已出版 - 15 8月 2025

学术指纹

探究 'Ablation behavior of UHTCs carbide-modified C/C composites in extreme aerobic environments (3000℃): Evolution mechanisms of oxides film structure' 的科研主题。它们共同构成独一无二的学术指纹。

引用此