摘要
Severe-plastic deformation (SPD) is a key approach to prepare high-performance Cu-Ni-Mn alloys by promoting θ-MnNi precipitation and inducing α-Cu grain refinement, but it is not practical to produce components with complex geometries. Here, Cu-20wt.%Ni-20wt.%Mn alloy with high strength up to 1345 MPa and 3.6% tensile ductility was fabricated by ultrasonic solidification and subsequent heat treatment without any deformation procedures, whose comprehensive mechanical property was even better than those after SPD. Ultrasound transformed coarse α-Cu dendrites into tiny equiaxed grains, with homogenized solutes and high dislocation density after solidification. These further provided abundant nucleation sites and reduced solute concentration gradient during subsequent heat treatment, facilitating the precipitation of θ-MnNi phase with small size and increased volume fraction. The effective precipitation and grain refinement enhanced alloy strength, while dense slipping dislocations and deformation twins improved its plasticity, which both contributed to the strength-ductility synergy.
| 源语言 | 英语 |
|---|---|
| 期刊论文编号 | 117555 |
| 期刊 | Scripta Materialia |
| 卷 | 287 |
| DOI | |
| 出版状态 | 已出版 - 15 1月 2027 |
学术指纹
探究 'A synergetic enhancement of strength and ductility for Cu-Ni-Mn alloy through ultrasonic modulation' 的科研主题。它们共同构成独一无二的学术指纹。引用此
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver