Nickel-based single crystal superalloys have been widely used in modern aircraft, which is related to its high temperature mechanical strength and creep properties. And the initial cubic ?' precipitates start to coarsen directionally during high temperature creep, which results in the degradation of the mechanical properties, especially the creep properties. Therefore, it is essential to figure out the mechanism of directional coarsening during the period of high temperature creep. In this article, a broad review of rafting mechanism of nickel-based single crystal superalloys is provided. The major work of this critical review is to introduce several experiments and numerical simulations which are used to analyze the evolution of rafting. For three different numerical simulations, their performance, advantage and disadvantage are discussed in detail. Through methods above, the effect on creep properties is summarized.

源语言英语
主期刊名Functional Materials and Metallurgy - ICFMM 2016
编辑Haider F. Abdul Amir
出版商Trans Tech Publications Ltd
41-49
页数9
ISBN(印刷版)9783035711110
DOI
出版状态已出版 - 2017
活动International Conference on Functional Materials and Metallurgy, ICFMM 2016 - Shanghai, 中国
期限: 3 8月 20165 8月 2016

出版系列

姓名Solid State Phenomena
263 SSP
ISSN(印刷版)1012-0394
ISSN(电子版)1662-9779

会议

会议International Conference on Functional Materials and Metallurgy, ICFMM 2016
国家/地区中国
Shanghai
时期3/08/165/08/16

指纹

探究 'A review of rafting in nickel-based single crystal superalloys' 的科研主题。它们共同构成独一无二的指纹。

引用此