TY - JOUR
T1 - A dimensionless nanoindentation-based inverse framework for identifying Johnson–Cook constitutive parameters in Sn-based solder materials
AU - Shen, Ziyi
AU - Siow, Kim Shyong
AU - Wang, Shaoxi
AU - Long, Xu
N1 - Publisher Copyright:
© 2026 Elsevier Ltd
PY - 2027/2
Y1 - 2027/2
N2 - Sn-based solder materials exhibit nonlinear elastoplastic behavior and strain-rate sensitivity at small scales, making constitutive parameter identification highly challenging. Conventional nanoindentation-based inverse analyses relying solely on load–penetration depth (P–h) curves often suffer from parameter coupling and non-uniqueness, where distinct constitutive parameter sets may produce nearly identical indentation responses. To address this issue, a dimensionless inverse framework is proposed to identify Johnson–Cook constitutive parameters based on nanoindentation responses. A representative parameter range is constructed based on typical Sn-based solder materials, and extensive finite element simulations are performed to generate a response database. Through dimensional analysis, a generalized function is established between multi-depth P–h data and constitutive parameters, improving the robustness of parameter identification. Furthermore, the depth-dependent hardness evolution is incorporated as an additional constraint to improve parameter identifiability, reflecting combined viscoplastic and scale effects. The results demonstrate that materials exhibiting similar P–h curves can be effectively distinguished through their differences in hardness evolution and characteristic length, thereby alleviating the non-uniqueness issue in the inverse analysis. The proposed framework requires only P–h data without additional experimental measurements, providing an efficient and practical approach for in-situ constitutive characterization of Sn-based solder materials.
AB - Sn-based solder materials exhibit nonlinear elastoplastic behavior and strain-rate sensitivity at small scales, making constitutive parameter identification highly challenging. Conventional nanoindentation-based inverse analyses relying solely on load–penetration depth (P–h) curves often suffer from parameter coupling and non-uniqueness, where distinct constitutive parameter sets may produce nearly identical indentation responses. To address this issue, a dimensionless inverse framework is proposed to identify Johnson–Cook constitutive parameters based on nanoindentation responses. A representative parameter range is constructed based on typical Sn-based solder materials, and extensive finite element simulations are performed to generate a response database. Through dimensional analysis, a generalized function is established between multi-depth P–h data and constitutive parameters, improving the robustness of parameter identification. Furthermore, the depth-dependent hardness evolution is incorporated as an additional constraint to improve parameter identifiability, reflecting combined viscoplastic and scale effects. The results demonstrate that materials exhibiting similar P–h curves can be effectively distinguished through their differences in hardness evolution and characteristic length, thereby alleviating the non-uniqueness issue in the inverse analysis. The proposed framework requires only P–h data without additional experimental measurements, providing an efficient and practical approach for in-situ constitutive characterization of Sn-based solder materials.
KW - Inverse algorithm
KW - Johnson–cook constitutive model
KW - Nanoindentation
KW - Non-uniqueness
KW - Sn-based solder materials
UR - https://www.scopus.com/pages/publications/105052138063
U2 - 10.1016/j.mssp.2026.111228
DO - 10.1016/j.mssp.2026.111228
M3 - 文章
AN - SCOPUS:105052138063
SN - 1369-8001
VL - 218
JO - Materials Science in Semiconductor Processing
JF - Materials Science in Semiconductor Processing
M1 - 111228
ER -