Abstract
A multilayered ((Nb,Cr,Ti)Si2+Cr4Nb2Si5)/NbSi2 composite coating was fabricated on Nb521 alloy via slurry sintering. The oxidation behavior of the coating was systematically investigated over the temperature range of 1200–1500 °C. The results indicated that the outward diffusion of Cr is dominant in the early stage of oxidation, leading to the formation of Cr2O3 as the primary oxidation product with minor SiO2. During the later oxidation stage, Si outward diffusion becomes predominant, resulting in SiO2 and TiO2 as the main oxidation products. At 1200 °C and 1300 °C, the scale is prone to peeling off due to the slow formation rate and poor fluidity of SiO2. In contrast, at 1400–1500 °C, the enhanced fluidity of SiO2 enables effective sealing of pores and cracks, resulting in superior oxidation resistance of the coating. As the temperature increased, the degradation of the (Nb,Cr,Ti)Si2, Cr4Nb2Si5, and NbSi2 phases in the coating was accelerated, driven by the outward diffusion of Si and Cr as well as the inward Si diffusion into the substrate. The growth kinetics of the interdiffusion zone (IDZ) followed a parabolic law, and the activation energy ( E ₐ) for Nb5Si3 layer was calculated as 222.82 kJ/mol.
| Original language | English |
|---|---|
| Article number | 108689 |
| Journal | Surfaces and Interfaces |
| Volume | 86 |
| DOIs | |
| State | Published - 1 Apr 2026 |
Keywords
- Nb based alloy
- NbSi
- Oxidation behavior
- Silicide coating
- Slurry sintering
Fingerprint
Dive into the research topics of 'Temperature-dependent oxidation behavior and interfacial diffusion dynamics of multilayered silicide coating on Nb521 alloy (1200-1500 °C)'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver