Abstract
Forsterite (Mg2SiO4) microwave dielectric ceramics exhibit low relative permittivity and low dielectric loss, making them promising materials for high-frequency communication devices. Building on the reported suppressive effect of Mg-excess compositions on the formation of the MgSiO3 secondary phase, Mg2.05SiO4 was selected as the base matrix in this study. On this basis, Ca2 + doping and CaTiO3 composite compensation were combined to achieve synergistic regulation of the structure, dielectric loss, and temperature stability. The optimized 0.96Mg2.05Ca0.08SiO4-0.04CaTiO3 ceramic has ε r = 7.49 ± 0.20, Q×f = 94563 ± 3000 GHz @12.87 GHz, and τ f = -3.86 ± 3.00 ppm/°C. The positive shift of τ f with Ca2+ incorporation correlates with the reduced distortion of the local Mg/Ca-O coordination environment, while CaTiO3 further compensates the residual negative temperature drift. These results demonstrate a viable route to balancing low relative permittivity, low dielectric loss, and near-zero τ f in Mg2SiO4-based microwave dielectric ceramics.
| Original language | English |
|---|---|
| Article number | 118900 |
| Journal | Journal of the European Ceramic Society |
| Volume | 47 |
| Issue number | 3 |
| DOIs | |
| State | Published - Mar 2027 |
Keywords
- Composite modification
- MgSiO
- Microwave dielectric ceramics
- P-V-L theory
Fingerprint
Dive into the research topics of 'Synergistic microwave dielectric performance regulation of Mg2SiO4-based ceramics'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver