Abstract
Generating experimentally realistic superalloy microstructures from simulated cooling histories remains challenging because simulated thermal histories and experimentally characterized microstructures are linked by an imperfect simulation-to-experiment mapping. Can generative prediction remain reliable when conditioning descriptors predicted from simulated thermal histories deviate from their experimentally measured counterparts? Here, we establish a descriptor-mediated, mode-aware conditional diffusion framework that maps simulated thermal histories to experimentally derived microstructural descriptors and constrains diffusion trajectories using data-driven statistical mode labels. Mode-aware supervision provides the largest improvement among the ablated modules, improving six quantitative metrics—including distribution MAPE, KS statistic, Wasserstein distance, two-point correlation errors (L1 and L2), and microstructure error—by an average of 47.4%. A residual-perturbation strategy further quantifies the propagation of simulation-to-experiment mapping errors. Although degradation follows a super-linear power law (b ≈ 1.39), practical descriptor-level mapping errors cause only 0.724% microstructure-consistency degradation. The proposed framework enables robust generative superalloy microstructure prediction under descriptor-level simulation-to-experiment mapping errors.
| Original language | English |
|---|---|
| Article number | 117627 |
| Journal | Scripta Materialia |
| Volume | 288 |
| DOIs | |
| State | Published - 1 Feb 2027 |
| Externally published | Yes |
Keywords
- Microstructure prediction
- Mode-aware conditional diffusion
- Simulation-to-experiment mapping errors
- Solidification
- Superalloy
Fingerprint
Dive into the research topics of 'Robust generative superalloy microstructure prediction under simulation-to-experiment mapping errors via mode-aware conditional diffusion'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver