Preparation and properties of green crosslinked styrene butadiene rubber with poly (Malic Acid)

  • Changjie Yin
  • , Yibo Wu
  • , Huimin Li
  • , Dezhong Yin
  • , Qiuyu Zhang
  • Northwestern Polytechnical University Xian

Research output: Contribution to journal › Article › peer-review

Abstract

Nowadays, the most widely used vulcanization system for industrial rubber products is the traditional sulfur vulcanization system, which releases harmful gases and makes unsustainability for the development of rubber industry. Herein. In this study, the novel poly(Malic Acid) (PMA) is prepared by direct polymerization, the structure of PMA was confirmed by FTIR and 1HNMR, weight average molecular thermal stability of PMA is 4860 g/mol and 214 °C. Based on prepared EESBR with (Epoxidized emulsion styrene butadiene rubber) different epoxidized degrees, it was cured by PMA. It was found that PMA cured EESBR exhibits typical vulcanization behavior, with the increase of PMA addition, the crosslinking density increased to 9.39 × 10− 4 mol/cm3, and the tensile strength of PMA/EESBR gradually increased to 2.82 MPa, maximum torque (MH) can reach to 4.70 N*m. The value of tanδ at 60 °C and 0 °C are 0.0215 and 0.8625 respectively, exhibiting high wet skid resistance and low rolling resistance as a green tire tread. After one reprocessing properties of EESBR/PMA, the recovery rate is only 50%, it indicates that the crosslinked bonds in EESBR/PMA have not only dynamic hydroxyl ester bonds, but also irreversible ether bonds.

Original languageEnglish
Article number375
JournalJournal of Polymer Research
Volume33
Issue number9
DOIs
StatePublished - Sep 2026

Keywords

  • Green crosslinked
  • Poly malic acid
  • Rubber
  • β-hydroxy ester bonds

Fingerprint

Dive into the research topics of 'Preparation and properties of green crosslinked styrene butadiene rubber with poly (Malic Acid)'. Together they form a unique fingerprint.

Cite this