Orientation Characteristics of Single Crystal Superalloys with Different Preparation Methods

  • Chubin Yang
  • , Lin Liu
  • , Ning Luo
  • , Baojun Han
  • , Xiaolian Zhang
  • , Jun Zhang
  • , Hengzhi Fu
  • Northwestern Polytechnical University Xian
  • Gannan Normal University

Research output: Contribution to journalArticlepeer-review

6 Scopus citations

Abstract

Single crystal superalloys have been prepared separately by a grain selector and a seeding technique in a high temperature gradient directional solidification furnace. The orientation characteristics were measured by XRD. Results indicate that for the grain selector method, the crystal solidification begins at the cooling plate with random nucleation, and through mutual competitive growth at the starter block. The grains enter the spiral selector, and finally the single crystal superalloys which are close to <001> direction are obtained. By the seeding technique, by epitaxial growth of partially melted seed crystals, single crystal superalloys which have the same orientation as the seed crystal are obtained.

Original languageEnglish
Pages (from-to)912-916
Number of pages5
JournalXiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
Volume46
Issue number4
StatePublished - 1 Apr 2017

Keywords

  • Crystal orientation
  • Directional solidification
  • Grain selector
  • Seeding technique
  • Single crystal superalloys