Abstract
The function of AlF3 activator, the aluminized coating formation mechanism on K447A nickel-based superalloy during the pack cementation process, and their oxidation behaviors have been systematically investigated. Comprehensive characterization by XRD, SEM, TEM and EDS analyses with HSC thermochemical calculation reveals four key findings: AlF3 demonstrates the optimal aluminizing capability and generates active Al atoms via the disproportionation reaction of AlF gas. The aluminized coating exhibits a multilayer structure, with the outer layer composed of high Al content Ni2Al3 or NiAl3 and the inner layer consisting of NiAl. Precipitated phases such as α-(Cr, W), σ phase, and carbides are distributed in the aluminides, confirming an Al-dominated inward diffusion mechanism characteristic of a “high-activity” process. The coating thickness exhibits linear relationships to the reciprocal of temperature and holding time. Ni₂Al₃ is formed before NiAl, transforms into NiAl, and then is regenerated. After oxidizing at 1150 °C for 100 h, a protective ridged α-Al2O3 scale forms on the aluminide coating, effectively shielding the substrate.
| Original language | English |
|---|---|
| Article number | 132236 |
| Journal | Surface and Coatings Technology |
| Volume | 510 |
| DOIs | |
| State | Published - 15 Aug 2025 |
Keywords
- AlF activator
- K447A nickel-based superalloy
- Oxidation behavior
- Pack cementation aluminizing
- Thermodynamic analysis
Fingerprint
Dive into the research topics of 'Microstructure and oxidation behavior of the aluminized coating on K447A nickel-based superalloy prepared by AlF3-activated pack cementation'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver