The microstructure evolution and mechanical property of Ti-22Al-25Nb (at%) alloy by different phase region isothermal forging and heat treatment were studied. The results indicate that as the isothermally forging temperature increases from 980℃ (α2+O+B2 three phase region) to 1040℃ (α2+B2 two phase region) to 1060℃ (B2 phase region), the microstructures of alloys are equiaxed microstructure, duplex microstructure, and bimodal size lamellar O microstructure. The size and volume fraction of each phase can be controlled by heat-treatment schedule. The mechanical properties of alloys show that bimodal size lamellar O microstructure has the highest strength but the worst ductility; however, the equiaxed microstructure has the highest ductility but the lowest strength. The equiaxed microstructure has the worst creep resistance, while the duplex microstructure and the bimodal size lamellar O microstructure have similar creep resistance, because they are both mainly lamellar structure, which possess better creep resistance than the equiaxed microstructure.

Original languageEnglish
Pages (from-to)1605-1608
Number of pages4
JournalXiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering
Volume45
Issue number6
StatePublished - 1 Jun 2016

Keywords

  • Creep
  • Isothermal forging
  • Microstructure
  • Tensile
  • Ti-22Al-25Nb alloy

Fingerprint

Dive into the research topics of 'microstructure and mechanical properties of the isothermally forged Ti-22Al-25Nb (at%) alloy'. Together they form a unique fingerprint.

Cite this