Microstructural refinement of Ni-Cr-W superalloy by isothermal treatment near the liquidus

  • Northwestern Polytechnical University Xian
  • Xi'an University of Science and Technology

Research output: Contribution to journal › Article › peer-review

8 Scopus citations

Abstract

The solidification process of Ni-Cr-W superalloy was investigated by confocal scanning laser microscope (CSLM). The liquid fraction during solidification was obtained as a function of real time and temperature in reference with the in-situ observation. In this work, the effect of isothermal treatment near the liquidus on undercooling, grain initiation and the grain growth was studied, and an analytical model is developed to account for the effect of solute field on grain refinement. This study revealed that isothermal treatment near the liquidus restricted the growth of crystal and increased the number density of active particles for nucleation, giving rise to a finer grain size. The tensile results of Ni-Cr-W superalloy tested at different temperatures indicated fine grain microstructure can improve the mechanical properties at different temperatures.

Original languageEnglish
Pages (from-to)271-274
Number of pages4
JournalMaterials Letters
Volume175
DOIs
StatePublished - 15 Jul 2016

Keywords

  • Crystal growth
  • Isothermal treatment
  • Mechanical properties
  • Microstructure
  • Superalloy