Long-term water-oxygen corrosion behavior and mechanism of an all-oxide Yb-Al-Si-O glass-modified Yb2Si2O7 bond coat on SiCf/SiC composites at 1400 °C

  • Chun Guo
  • , Yujie Chen
  • , Yujie Ma
  • , Jianfeng Li
  • , Muzhen Jin
  • , Juanli Deng
  • , Shangwu Fan
  • Northwestern Polytechnical University Xian
  • Xi'an Modern Chemistry Research Institute
  • Chang'an University

Research output: Contribution to journal › Article › peer-review

Abstract

The long-term water-oxygen corrosion behavior of a Yb-Al-Si-O glass-modified Yb2Si2O7 coating on SiCf/SiC composites (A-D-SS) was investigated at 1400 °C for 200 h in 50 vol% H2O-50 vol% O2. A-D-SS exhibited continuous net mass gain with a decreasing rate, governed by water-vapor incorporation, limited SiC oxidation, and Si(OH)4 volatilization. At the surface, hydrolysis and volatilization of residual YbAS glass caused Si depletion and compositional rearrangement, promoting mullite enrichment and increasing surface roughness. Independently, corrosion-induced Si loss from Yb2Si2O7 grain boundaries produced a small amount of Yb2SiO5. Within the coating, localized penetration increased porosity, but no continuous transport pathways formed. At the coating/substrate interface, limited SiC oxidation produced amorphous SiO2, while residual YbAS glass underwent local crystallization, contributing to the formation of a nanoscale multiphase interfacial structure. Overall, A-D-SS retained structural integrity and effectively restricted sustained water-oxygen penetration, demonstrating its potential as an all-oxide bond coat for SiCf/SiC composites.

Original languageEnglish
Article number114353
JournalCorrosion Science
Volume273
DOIs
StatePublished - Dec 2026

Keywords

  • All-oxide bond coats
  • SiC/SiC composites
  • Water-oxygen corrosion
  • Yb-Al-Si-O glass

Fingerprint

Dive into the research topics of 'Long-term water-oxygen corrosion behavior and mechanism of an all-oxide Yb-Al-Si-O glass-modified Yb2Si2O7 bond coat on SiCf/SiC composites at 1400 °C'. Together they form a unique fingerprint.