Skip to main navigation Skip to search Skip to main content

Investigation on the oxidation and ablation behaviors of HfB2-SiC-Si/SiC-Si coatings for carbon/carbon composites

  • Lei Zhou
  • , Jiaping Zhang
  • , Dou Hu
  • , Qiangang Fu
  • , Jian Zhu
  • , Jingyuan Song
  • , Wuqing Ding
  • , Jiaqi Hou
  • , Mingde Tong
  • Northwestern Polytechnical University Xian
  • AECC Shenyang Engine Research Institute

Research output: Contribution to journal › Article › peer-review

44 Scopus citations

Abstract

Oxidation and ablation behaviors of HfB2-SiC-Si/SiC-Si coatings fabricated by dipping-carbonization joint gaseous silicon infiltration on cubic and nose-shaped carbon/carbon substrates were investigated. After 30 thermal cycles between 1500 °C and room temperature, the mass gain of the coated sample was 0.91 %, and the mass gain was 2.62 % after oxidation at 1500 °C for 870 h. The coated nose-shaped sample exhibited good anti-ablation properties at 1800 °C–2000 °C under oxyacetylene flame. Especially at 1800 °C, the mass ablation rate was −0.073 mg/s. Although the nose tip suffered the most serious corrosion, HfO2 scale surrounded by Hf-Si-O glass could withstand the oxyacetylene torch scouring.

Original languageEnglish
Article number109638
JournalCorrosion Science
Volume190
DOIs
StatePublished - Sep 2021

Keywords

  • Ablation behavior
  • C/C composites
  • HfB
  • Oxidation resistance

Fingerprint

Dive into the research topics of 'Investigation on the oxidation and ablation behaviors of HfB2-SiC-Si/SiC-Si coatings for carbon/carbon composites'. Together they form a unique fingerprint.

Cite this