In-situ SEM/DIC analysis of crack propagation path selection in TiAl/Ti2AlNb laminated composites: Pre-notch positioning dictates the fracture toughness in three-point bending tests

  • Beibei Wei
  • , Bin Tang
  • , Chenglin Li
  • , Xiang Zhang
  • , Biao Ma
  • , Xiangyu Pan
  • , Songkuan Zhao
  • , Xiaofei Chen
  • , Jinhua Dai
  • , Lei Zhu
  • , Jinshan Li
  • Xi'an Shiyou University
  • Northwestern Polytechnical University Xian
  • China National Petroleum Corporation
  • Xi'an University of Technology

Research output: Contribution to journal › Article › peer-review

Abstract

TiAl/Ti2AlNb laminated composites were fabricated by vacuum hot-pack rolling, forming three distinct interfacial regions: brittle regions I (βo + α2 + γ + ω) and II (βo/B2 + α2 + ω), and ductile region III (O). Multiscale characterization combining digital image correlation and in-situ three-point bending tests revealed that the laminated composites exhibit a 2.0–2.5-fold improvement in fracture toughness compared with monolithic TiAl alloy. This enhancement arises from the synergy between intrinsic and extrinsic toughening mechanisms. The intrinsic toughening is associated with slip deformation of B2 grains in the Ti2AlNb layer and grain-boundary obstruction to crack propagation, whereas the extrinsic toughening originates from interfacial crack branching in regions I and II, together with crack deflection and blunting in region III. Furthermore, the critical role of the pre-notch position was emphasized. When the notch terminates in the Ti2AlNb layer, interfacial crack branching effectively alleviates stress concentration, increasing KQ to 40.2 MPa m1/2. Conversely, when the notch terminates in the TiAl layer, rapid crack initiation caused by the low damage tolerance of TiAl triggers premature structural instability, reducing KQ to 29.5 MPa m1/2. These findings provide guidance for interfacial design and toughening optimization of TiAl-based laminated composites.

Original languageEnglish
Pages (from-to)303-313
Number of pages11
JournalJournal of Materials Science and Technology
Volume285
DOIs
StatePublished - 1 Apr 2027

Keywords

  • Crack propagation
  • In-situ three-point bending
  • Interfacial phase transformation
  • Strengthening and toughening mechanism
  • TiAl/TiAlNb laminated composites