Grain refinement of superalloy K4169 by addition of refiners: Cast structure and refinement mechanisms

  • Lin Liu
  • , Taiwen Huang
  • , Yuhua Xiong
  • , Aimin Yang
  • , Zhilong Zhao
  • , Rong Zhang
  • , Jinshan Li
  • Northwestern Polytechnical University Xian
  • General Research Institute for Non-ferrous Metals China
  • Xi'an Shiyou University

Research output: Contribution to journalArticlepeer-review

81 Scopus citations

Abstract

Grain size and microstructural features of cast superalloy K4169 were investigated under various melting and casting conditions with and without the addition of grain refiners. It is found that lowering pouring temperature and adding refiners to the melt can lead to grain refinement of γ matrix and improve the proportion of equiaxed grains. At a conventional pouring temperature of 1400 °C, the average size of equiaxed grains could be refined to the order of ASTM 3.2, the proportion of equiaxed grains at transverse cross-section could be improved from 56 to 99%. The results also indicate that the average length of primary dendrite axis is shortened with the addition of refiners, but the secondary dendrite arm spacing keeps almost unchanged because local solidification time remained constant. In addition, the microsegregation of main elements such as Fe, Cr, Nb, Mo and Ti is alleviated with the decrease in grain size, and the grain morphology have transformed from dendrite in coarse- to granulate in fine-grained castings. At higher melt pouring temperature, the amount of microporosity in samples with the addition of refiners can be greatly reduced. The mechanisms of grain refinement and increase in equiaxed grain proportion were proposed.

Original languageEnglish
Pages (from-to)1-8
Number of pages8
JournalMaterials Science and Engineering: A
Volume394
Issue number1-2
DOIs
StatePublished - 15 Mar 2005

Keywords

  • Dendrite structure
  • Grain refinement
  • Grain size
  • Microporosity
  • Microsegregation
  • Solidification
  • Superalloy