Abstract

Introducing high and deep compressive residual stress (CRS) through gradient plastic strain by surface strengthening technologies improves the fretting fatigue life of titanium alloys, but the effects of deformation mechanisms on CRS remain unclear. In this study, the high (-713 MPa) and deep (1148 μm) CRS was achieved in TB6 alloy by laser shock peening (LSP) and subsequent shot peening (SP) via sequential plasticity mechanisms in the primary α (αp), secondary α (αs), and β phases, indicating a superior CRS magnitude-depth balance over other surface strengthening technologies. The high CRS originates from dislocation multiplication in the αp, αs, and β phases, and {101¯1}<101¯2¯> twins in the αs phase induced by LSP, as well as higher dislocation density in the αp, αs, and β phases, and {101¯2}<1¯011> twins in the αp phase induced by SP. Meanwhile, the deep CRS results from large penetration depth of shock waves and plastic strain during LSP. Crystal plasticity simulations reveal that high strain rate and large strain under combined LSP and SP promote the activation of {101¯2}<1¯011> and {101¯1}<101¯2¯> twinning of α phase, enhancing the plastic strain and CRS. Besides, phase morphology and size govern twinning modes in the αs and αp phases, while stacking faults further facilitate {101¯2}<1¯011> twinning. Sequential plasticity mechanisms also induce surface-to-interior gradient microstructure, and the synergy of CRS and gradient microstructure increases the fretting fatigue life to beyond 2 × 106 cycles under a maximum stress of 125 MPa and a stress ratio of 0.06, over 13-fold that of the untreated alloy.

Original languageEnglish
Article number104731
JournalInternational Journal of Plasticity
Volume203
DOIs
StatePublished - Aug 2026

Keywords

  • Fretting fatigue
  • Laser shock peening
  • Residual stress
  • Sequentially activated plasticity mechanism
  • Shot peening
  • TB6 titanium alloy

Fingerprint

Dive into the research topics of 'Enhancing surface compressive residual stress and its depth in TB6 alloy via sequentially activated plasticity mechanisms for exceptional fretting fatigue life'. Together they form a unique fingerprint.

Cite this