Enhanced thermoelectric performance in p-type AgBiSe2 through carrier concentration optimization and valence band modification

Hao Ming Liu, Xiu Qun Wu, Jia Yan Sun, Shan Li, Jun Xiong Zhang, Xin Li Ye, Qian Zhang

Research output: Contribution to journalArticlepeer-review

Abstract

Realizing the high thermoelectric performance of p-type AgBiSe2-based materials has been challenging due to their low p-type dopability. This work demonstrated that Cd doping at the Bi site converts n-type AgBiSe2 to p-type. The hole concentration is effectively increased with increasing Cd doping content, thereby enhancing the electrical conductivity. Theoretical calculations reveal that Cd doping flattens the edge of the valence band, resulting in an increase in the density-of-states effective mass and Seebeck coefficient. A record-high power factor of ~ 6.2 µW⋅cm−1⋅K−2 was achieved at room temperature. Furthermore, the induced dislocations enhance the phonon scattering, contributing to the ultralow lattice thermal conductivity across the entire temperature range. As a result, a decent figure of merit (zT) of ~ 0.3 at room temperature and a peak zT of ~ 0.5 at 443 K were obtained in AgBi0.92Cd0.08Se2. Our work provides a feasible method for optimizing the thermoelectric performance of p-type AgBiSe2. Graphical Abstract: (Figure presented.)

Original languageEnglish
JournalRare Metals
DOIs
StateAccepted/In press - 2024

Keywords

  • AgBiSe
  • Cd doping
  • P-type
  • Thermoelectric

Fingerprint

Dive into the research topics of 'Enhanced thermoelectric performance in p-type AgBiSe2 through carrier concentration optimization and valence band modification'. Together they form a unique fingerprint.

Cite this