Skip to main navigation Skip to search Skip to main content

Damage evolution mechanism around AlN non-metallic inclusions in Fe-8.5Mn–3Al-0.2C lightweight medium-Mn steel during warm forming

  • Y. Sun
  • , X. L. Li
  • , X. Z. Liu
  • , H. L. Hou
  • , K. Xie
  • , L. F. He
  • , Z. C. Li
  • , H. P. Li
  • Shandong University of Science and Technology
  • Northwest Institute for Nonferrous Metal Research

Research output: Contribution to journalArticlepeer-review

7 Scopus citations

Abstract

Based on the tensile test in two-phase region, the damage evolution mechanism around AlN non-metallic inclusions in Fe-8.5Mn–3Al-0.2C lightweight medium-Mn steel during warm forming was elucidated. The findings indicate that voids primarily originate from the bonding interfaces between AlN non-metallic inclusions and ferrite. According to the numerical simulation results, strain eventually concentrates at the bonding interface where the AlN inclusion is connected to the high-strain ferrite in the direction parallel to the load, which is in good agreement with the experimental results. TEM analysis reveals the semi-coherent interface between AlN and austenite as well as the incoherent interface between AlN and ferrite. The incoherent interface between AlN and ferrite exhibits higher interfacial energy and worse mechanical stability, accelerating the separation of the bonding interface between AlN and ferrite.

Original languageEnglish
Article number146456
JournalMaterials Science and Engineering: A
Volume899
DOIs
StatePublished - May 2024
Externally publishedYes

Keywords

  • AlN non-metallic inclusion
  • Bonding interface
  • Damage evolution
  • Medium-Mn steel
  • Numerical simulation
  • Warm forming

Fingerprint

Dive into the research topics of 'Damage evolution mechanism around AlN non-metallic inclusions in Fe-8.5Mn–3Al-0.2C lightweight medium-Mn steel during warm forming'. Together they form a unique fingerprint.

Cite this