Abstract
This work investigates the high-temperature compressive creep response of a ZrB₂/SiC composite fabricated by reactive spark plasma sintering from B₄C, Zr₅Si₃, and carbon precursors. The process produced a dense two-phase composite consisting of ZrB₂ and SiC, with a fine hierarchical microstructure in which SiC occurred as intergranular regions and fine intragranular inclusions. Compressive creep tests were performed at 1300–1400°C under stresses of 100–200 MPa. The composite showed good short-term creep resistance at 1300°C, whereas testing at 1400°C under 100 MPa led to a marked increase in recorded strain and apparent late-stage creep rate. SEM observations after the 1400°C test revealed extensive cracking and local decohesion associated mainly with SiC-rich regions and ZrB₂/SiC interfaces. Thermal-stress analysis indicated that thermal-expansion mismatch between ZrB₂ and SiC contributed to damage-assisted deformation at 1400°C.
| Original language | English |
|---|---|
| Article number | 118883 |
| Journal | Journal of the European Ceramic Society |
| Volume | 47 |
| Issue number | 3 |
| DOIs | |
| State | Published - Mar 2027 |
Keywords
- Composite
- Creep resistance
- Microstructure
- Silicon carbide
- Zirconium diboride
Fingerprint
Dive into the research topics of 'Creep resistance limits of ZrB2/SiC composite reactively sintered from B4C and Zr5Si3 precursors'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver