Abstract
This study systematically investigates the microstructural evolution, analyzing coarsening and grain growth kinetics of the Ni32.5Co15Cr10Fe23Al17.5Mo1.5W0.5 eutectic high-entropy alloy (EHEA) fabricated by selective laser melting (SLM) during annealing at 1100 °C (up to 360 h). The cellular structure evolved differently on the two principal planes. On the plane perpendicular to the building direction (⊥BD), the cells transformed into laths. On the plane parallel to the building direction (∥BD), the elongated cells evolved into elongated laths that subsequently widened, developed grooves, and partially spheroidized. Coarsening on both planes was controlled by grain-boundary diffusion. Grain boundaries were randomly oriented on the ⊥BD plane but were denser and mainly aligned with the building direction on the ∥BD plane. The resulting increase in effective diffusion efficiency produced faster coarsening on the ∥BD plane. The FCC grain-growth exponent was approximately 4, as commonly reported for high-entropy alloys. However, the FCC grain-growth rate constants differed only slightly between the two planes, indicating that FCC grain growth was less sensitive to grain-boundary density and distribution than two-phase coarsening. These findings clarify the anisotropic coarsening of an SLM-fabricated FCC/B2 EHEA and provide a basis for assessing its microstructural stability during prolonged high-temperature exposure.
| Original language | English |
|---|---|
| Article number | 109543 |
| Journal | Intermetallics |
| Volume | 198 |
| DOIs | |
| State | Published - Nov 2026 |
Keywords
- Coarsening kinetics
- Eutectic high-entropy alloys
- Grain-boundary diffusion
- Selective laser melting
Fingerprint
Dive into the research topics of 'Coarsening anisotropy of an SLM-fabricated FCC/B2 eutectic high-entropy alloy during prolonged annealing'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver