Bending-dominated miniature creep testing: A synthesis of theory and practice

  • University of Nottingham
  • East China University of Science and Technology
  • Northwestern Polytechnical University Xian
  • Siemens Energy UK

Research output: Contribution to journal › Article › peer-review

Abstract

This paper presents a unified framework for interpreting miniature bending creep test data, encompassing simply supported beams, fixed beams, cantilever beams, and bending plates, through the systematic synthesis of previously developed formulations within a common reference-stress framework. Material-independent but geometry- and loading-mode-dependent conversion parameters (η,β) relate measured global displacement to equivalent uniaxial creep response, with the Equivalent Gauge Length (LEGL) providing a useful geometry-dependent metric for test sensitivity. Analytical solutions are compiled for plane-stress, plane-strain, and finite-width 3D conditions, together with corresponding load-line displacement-rate formulations. The framework is further extended to consider creep damage, large-deformation effects, and multilayer systems. Experimental comparisons support the applicability of the reference-stress conversion approach for the specific configurations and materials considered, while analytical and numerical extensions identify areas requiring further validation. A comparative selection matrix highlights the characteristics and practical considerations of different miniature bending configurations. The resulting framework provides a consistent basis for extracting creep properties from limited material volumes and supports high-temperature structural integrity assessment and life management.

Original languageEnglish
Article number113468
JournalResults in Engineering
Volume32
DOIs
StatePublished - Dec 2026

Keywords

  • Analytical solutions
  • Bending creep
  • Equivalent gauge length
  • Miniature creep testing
  • Reference stress method
  • Two-layer materials