Advance in research of casting defects of directionally solidified nickel-based single superalloys

  • Northwestern Polytechnical University Xian

Research output: Contribution to journalReview articlepeer-review

17 Scopus citations

Abstract

Casting defects are deleterious to the mechanical properties of nickel-based single superalloys, the decrease of casting defects is benefit for improving mechanical properties and reducing the cost. Some important casting defects formed in the directional solidification process are discussed, including porosity, freckles, misorientation and stray grains. Based on the features and formation mechanisms for the defects, the influence of alloy composition, processing parameters and casting structure on the casting defects is analyzed. Meanwhile, the suggestions for reducing casting defects are pointed out.

Original languageEnglish
Pages (from-to)93-98
Number of pages6
JournalCailiao Gongcheng/Journal of Materials Engineering
Issue number1
StatePublished - Jan 2012

Keywords

  • Casting defect
  • Directional solidification
  • Nickel-based single superalloy
  • Processing parameter