Skip to main navigation Skip to search Skip to main content

A synergetic enhancement of strength and ductility for Cu-Ni-Mn alloy through ultrasonic modulation

  • Qian Zhou
  • , Jianyuan Wang
  • , Yajie Hu
  • , Wei Zhai
  • , Bingbo Wei
  • Northwestern Polytechnical University Xian

Research output: Contribution to journal › Article › peer-review

Abstract

Severe-plastic deformation (SPD) is a key approach to prepare high-performance Cu-Ni-Mn alloys by promoting θ-MnNi precipitation and inducing α-Cu grain refinement, but it is not practical to produce components with complex geometries. Here, Cu-20wt.%Ni-20wt.%Mn alloy with high strength up to 1345 MPa and 3.6% tensile ductility was fabricated by ultrasonic solidification and subsequent heat treatment without any deformation procedures, whose comprehensive mechanical property was even better than those after SPD. Ultrasound transformed coarse α-Cu dendrites into tiny equiaxed grains, with homogenized solutes and high dislocation density after solidification. These further provided abundant nucleation sites and reduced solute concentration gradient during subsequent heat treatment, facilitating the precipitation of θ-MnNi phase with small size and increased volume fraction. The effective precipitation and grain refinement enhanced alloy strength, while dense slipping dislocations and deformation twins improved its plasticity, which both contributed to the strength-ductility synergy.

Original languageEnglish
Article number117555
JournalScripta Materialia
Volume287
DOIs
StatePublished - 15 Jan 2027

Keywords

  • Copper alloys
  • Isothermal heat treatment
  • Mechanical properties
  • Ultrasonic solidification

Fingerprint

Dive into the research topics of 'A synergetic enhancement of strength and ductility for Cu-Ni-Mn alloy through ultrasonic modulation'. Together they form a unique fingerprint.