Abstract
Sn-based solder materials exhibit nonlinear elastoplastic behavior and strain-rate sensitivity at small scales, making constitutive parameter identification highly challenging. Conventional nanoindentation-based inverse analyses relying solely on load–penetration depth (P–h) curves often suffer from parameter coupling and non-uniqueness, where distinct constitutive parameter sets may produce nearly identical indentation responses. To address this issue, a dimensionless inverse framework is proposed to identify Johnson–Cook constitutive parameters based on nanoindentation responses. A representative parameter range is constructed based on typical Sn-based solder materials, and extensive finite element simulations are performed to generate a response database. Through dimensional analysis, a generalized function is established between multi-depth P–h data and constitutive parameters, improving the robustness of parameter identification. Furthermore, the depth-dependent hardness evolution is incorporated as an additional constraint to improve parameter identifiability, reflecting combined viscoplastic and scale effects. The results demonstrate that materials exhibiting similar P–h curves can be effectively distinguished through their differences in hardness evolution and characteristic length, thereby alleviating the non-uniqueness issue in the inverse analysis. The proposed framework requires only P–h data without additional experimental measurements, providing an efficient and practical approach for in-situ constitutive characterization of Sn-based solder materials.
| Original language | English |
|---|---|
| Article number | 111228 |
| Journal | Materials Science in Semiconductor Processing |
| Volume | 218 |
| DOIs | |
| State | Published - Feb 2027 |
Keywords
- Inverse algorithm
- Johnson–cook constitutive model
- Nanoindentation
- Non-uniqueness
- Sn-based solder materials
Fingerprint
Dive into the research topics of 'A dimensionless nanoindentation-based inverse framework for identifying Johnson–Cook constitutive parameters in Sn-based solder materials'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver